1
Paul D Genereux, Daniel F Paulonis: Nickel base superalloy articles and method for making. United Technologies Corporation, September 6, 1988: US04769087 (22 worldwide citation)

A process is described for converting a fine grain superalloy casting into a forging having mechanical properties equivalent to those resulting from powder metallurgy processing. Cast material is extruded and forged. A HIP treatment is employed to close porosity.


2
Genereux Paul Damian, Paulonis Daniel Francis: Nickel base superalloy articles and method for making.. United Technologies, December 9, 1987: EP0248757-A1 (18 worldwide citation)

A process is described for converting a fine grain superalloy casting into a forging having mechanical properties equivalent to those resulting from powder metallurgy processing. Cast material is extruded and forged, A HIP treatment is employed to close porosity.


3
Genereux Paul Damian, Paulonis Daniel Francis: Articles en superalliage a base de nickel, et leur fabrication, Nickel base superalloy articles and method for making. United Technologies Corporation, OGILVY RENAULT SENCRLSRL, May 28, 1991: CA1284450

Abstract of the Disclosure Nickel Base Superalloy Articles And Method For Making A process is described for converting a fine grain superalloy casting into a forging having mechanical properties equivalent to those resulting from powder metallurgy processing. Cast material is extruded and forged. A ...


4
Daniel Francis Paulonis, Paul Damian Genereux: Nickel base superalloy articles and method for making. United Technologies, YANG LIQIN, December 16, 1987: CN87103970

A process is described for converting a fine grain superalloy casting into a forging having mechanical properties equivalent to those resulting from powder metallurgy processing. Cast material is extruded and forged, A HIP treatment is employed to close porosity.