Hakam Singh, Jack W Hutt: Method of producing mercaptan terminated polymers with increased reactivity and reduced odor. Products Research & Chemical, Poms Smith Lande & Rose, March 1, 1988: US04728712 (15 worldwide citation)

A method for producing mercaptan terminated liquid polymers with increased chemical reactivity and reduced odor is disclosed which involves heating the polymeric liquid material under conditions which avoid oxidation and depolymerization of the material while removing at least 50 weight percent of l ...


2
Singh Hakam, Hutt Jack W: Method of producing mercaptan terminated polymers with increased reactivity and reduced odor.. Prod Res & Chem, July 1, 1987: EP0226578-A1

A method for producing mercaptan terminated liquid polymers with increased chemical reactivity and reduced odor which involves heating the polymeric liquid material under conditions which avoid oxidation and depolymerization of the material while removing at least 50 weight percent of low molecular ...


3
Singh Hakam, Hutt Jack W: Methode de preparation de polymeres terminees par un mercaptan, a reactivite plus grande et a odeur reduite, Method of producing mercaptan terminated polymers with increased reactivity and reduced odor. Prc Desoto International, SIM & MCBURNEY, January 30, 1990: CA1265162

METHOD OF PRODUCING MERCAPTAN TERMINATED POLYMERS WITH INCREASED REACTIVITY AND REDUCED ODOR Abstract of the Disclosure A method for producing mercaptan terminated liquidpolymers with increased chemical reactivity and reducedodor is disclosed which involves heating the polymericliquid material under ...


4
Singh Hakam, Hutt Jack W: Method of producing mercaptan terminated polymers with increased reactivity and reduced odor. Products Research And Chemical Corporation, Singh Hakam, Hutt Jack W, LANDE Gary E, December 18, 1986: WO/1986/007369

A method for producing mercaptan terminated liquid polymers with increased chemical reactivity and reduced odor which involves heating the polymeric liquid material under conditions which avoid oxidation and depolymerization of the material while removing at least 50 weight percent of low molecular ...