Spin finish for yarns to be bonded to rubber includes polyvinyl alcohol and microcrystalline or emulsifiable polyethylene wax. The wax has a melting point of at least 50.degree. C. and a penetration at 77.degree. F. of between 1 and 10 in accordance with ASTM test method D-1321-55T.