05946550 is referenced by 8 patents and cites 6 patents.

A method for producing a ultrathin semiconducting film, utilizes a substrate with a reactive functionalized surface which is contacted with a reactant compound of a divalent and trivalent chelating metal to produce a metallo-functionalized surface. The metallo-functionalized surface is contacted with bisquinoline or a bisquinoline to produce a deposit of an oligomeric metallo-bisquinoline chelate, which is then contacted with the reactant metal compound to produce a fresh metallo-functionalized surface on the deposit. The fresh metallo-functionalized surface is contacted with the bisquinoline reactant to produce a further deposit of the oligomeric metallo-bisquinoline chelate, and these steps are repeated until a desired thickness of the deposit has been attained.

Title
Self-assembled semiconductor and method of making same
Application Number
8/818382
Publication Number
5946550
Application Date
March 14, 1997
Publication Date
August 31, 1999
Inventor
Fotios Papadimitrakopoulos
Coventry
CT, US
Agent
Pepe & Hazard
Assignee
University of Connecticut
CT, US
IPC
B23B 27/00
H01L 33/00
H01L 35/24
View Original Source