04761183 is referenced by 101 patents and cites 17 patents.

A grouting composition, a method of grouting and a formation so grouted are disclosed. The composition comprises a very small particle size slag, an equal or greater weight of water and the optional components cement, alkali silicate, anionic dispersant, a source of orthophosphate ions, sodium hydroxide and sodium carbonate. The grout is particularly adapted to the treatment of "tight" or low permeability formations being low in viscosity and having controllable set time and hardening time as well as high strength upon hardening. Being based on slag, a byproduct, the grout is economical.

Title
Grouting composition comprising slag
Application Number
7/4668
Publication Number
4761183
Application Date
January 20, 1987
Publication Date
August 2, 1988
Inventor
William J Clarke
162 Spencer Pl., Ridgewood, 07450
NJ, US
Agent
Harold L Greenwald
Assignee
William J Clarke
NJ, US
Geochemical Corporation
NJ, US
IPC
C01B 7/14
View Original Source