PURPOSE: To obtain tin oxide powder usable for producing conductive toner powder. CONSTITUTION: A stannic salt soln. is mixed with a fluoride soln., tin hydroxide is separated from the liq. and dried at a temp. not exceeding room temp. and the dried product is heated to at least 500°C until the fluorine content is reduced to

Title
Production of fluorine-doped tin oxide powder