A process for producing EP and EPDM polymers with a reduction in fouling is provided, which process comprises polyemrizing ethylene, an alpha-olefin and a nonconjugated diolefin (if utilized) in a polymerization medium comprising a hydrocarbon diluent at a temperature of from about -50 DEG C to about 150 DEG C in the presence of a catalyst system comprising (a) a vanadium compound, (b) diethyl aluminum chloride, ethyl aluminum sesquichloride or ethyl aluminum dichloride and (c) an organo aluminum compound of the formula R3Al wherein R is an alkyl group having from 8 to 12 carbon atoms and, optionally, triethyl aluminum, the molar ratio of chloride in diethyl aluminum chloride to the total aluminum content in (b) and (c) being from about 0.7:1 to about 0.95:; 1, the molar ratio of the chloride in ethyl aluminum sesquichloride to the total aluminum content in (b) and (c) being from about 0.7:1 to about 1.4:1 and the molar ratio of the chloride in ethyl aluminum dichloride to the total aluminum content in (b) and (c) being from about 0.7:1 to about 1.8:1 and the ratio of the mols of vanadium compound to the total mols of diethyl aluminum chloride and ethyl aluminum sesquichloride being from about 1:10 to about 1:50 to the desired conversion.

Title
Reduced fouling in process for production of ep.
Application Number
EP19940117016 19941027
Publication Number
0652234 (A2)
Application Date
October 27, 1994
Publication Date
May 10, 1995
Inventor
Padliya Dilipkumar
CA
Osman Akhtar
CA
Knauf Thomas F
CA
Assignee
Polysar Rubber
CA
IPC
C08F 210/18
C08F 210/16
C08F 04/68
C08F 210/00
C08F 10/00
C08F 04/00
C08F 02/04
C08F 02/00
C08F 210/16
C08F 10/00
C08F 04/68
C08F 04/655
C08F 04/60
C08F 02/06
C08F 02/00
View Original Source Download PDF